Billet vs Cast Aluminum: Strength, Weight and When to Switch to a Casting

Billet aluminum, usually 6061-T6 bar or plate, is stronger than cast aluminum such as A356 in yield strength and ductility. 6061-T6 extruded bar has minimums of 240 MPa yield and 10% elongation; A356.0-T61 permanent-mold test bars have 180 MPa and 4% (ASTM B108/B108M-19, SI table). Tensile minimums are both about 260 MPa. A casting pays off for cored or curved shapes, heavy chip loss and volume that covers the die.

Aisle between CNC machining centers with wire baskets and stacked aluminum castings, workers far back
On this page
  1. Billet vs cast aluminum: the quick answer
  2. Why is billet aluminum stronger than cast aluminum?
  3. Is billet or cast aluminum lighter?
  4. When does a casting cost less than a billet part?
  5. Should a billet part become a casting? A decision table
  6. What changes on the drawing when a billet part becomes a casting?
  7. What inspection does a casting need that a billet part does not?
  8. Converting a billet part at Bohua
  9. Billet vs cast aluminum: buyer questions
  10. Sources

Billet vs cast aluminum: the quick answer

  • Keep billet for prototypes, changing designs, or parts that need 240 MPa (35 ksi) yield or 10% elongation everywhere.
  • Switch to a casting for cored or curved shapes, heavy chip loss and steady annual volume.
  • Either way, casting minimums come from test bars, so the drawing must say what the part itself must prove.
6061-T6 bar vs A356 and A357 castings: specified minimums and typical values
Material, product and basisTensile strength, MPa (ksi)Yield strength, MPa (ksi)Elongation, %Density, g/cm³ (lb/in³)
6061-T6 extruded bar, 6.35 mm (0.250 in) and thicker, minimum260 (38)240 (35)102.70 (0.098), nominal
6061-T6, typical310 (45)276 (40)172.70 (0.098)
A356.0-T61 permanent mold, separately cast test bars, minimum260 (38)180 (26)4 (SI); 5 (inch-pound)2.66–2.68 (0.096–0.097), typical
A356 permanent mold, T6 or T61, typical (producer data)285–340 (41–49)205–280 (30–41)5–122.66–2.68 (0.096–0.097)
A357.0-T61 permanent mold, separately cast test bars, minimum310 (45)250 (36)3Not specified

Sources: Aluminum Association (AA) Table 11.1, June 2017 page, ksi limits converted to MPa (6061 bar); ASTM B108/B108M-19, SI table in MPa, inch-pound table in ksi (castings); producer data (typical). B108/B108M-25 is current; use the edition on your order. Elongation is in 50 mm (2 in) or 4D (B108 SI table: 5D).

"Billet" has two meanings. To an extruder, it is a cast log cut to length for the press. To machinists and buyers, and in this guide, a billet part is cut from solid wrought stock, usually 6061-T6 bar or plate. Plate and rolled bar have their own minimum tables.

Why is billet aluminum stronger than cast aluminum?

Billet is stronger because it is wrought: it was hot or cold worked after casting, while a casting keeps the structure it formed in the mold. The gap shows up in three places.

  • Where the minimum applies. The 6061-T6 limits apply to the bar you buy. The casting limits in ASTM B108 and EN 1706 apply to separately cast test bars poured with the parts.
  • What happens inside a real casting. Properties vary with section thickness and soundness. ASTM B108/B108M-19 sets separate cut-specimen minimums for A356.0 and A357.0; its default of 75% of test-bar strength and 25% of elongation covers other alloys, and B26 applies it to sand castings. EN 1706 leaves cut-specimen values to agreement between supplier and purchaser; strength may be as low as 70% of the table values, and elongation up to 50% lower in places.
  • Where fatigue cracks start. In A356-T6, fatigue cracks usually start at casting defects such as pores. Typical fatigue strength is 97 MPa (14 ksi) at 5×10⁸ cycles for 6061-T6 and 80–110 MPa (12–16 ksi) up to 10⁷ cycles for the A356 type in EN 1706; the bases differ, so do not rank them.

So the fair comparison is bar against the property you specify, and verify, in the critical zone of the casting. The T6 heat treatment and acceptance guide covers temper callouts and batch records.

Is billet or cast aluminum lighter?

At equal volume, an A356 casting is about 1% lighter than 6061 bar: about 2.66–2.68 g/cm³ against 2.70 g/cm³. Real weight differences come from section sizes, not from density.

  • Stiffness-limited parts. Elastic modulus is about the same: 68.9 GPa (10,000 ksi) for 6061-T6 and about 69–75 GPa for A356 (typical). A housing sized for deflection needs no extra wall for stiffness, but the casting process sets its own minimum wall.
  • Shape freedom. A casting can carry ribs, cored passages and hollow sections that no cutter can reach. That is where a redesigned casting wins weight back.

Worked example: converting a strength-limited arm

An illustrative cantilever arm is machined from 6061-T6 bar. Its root is a solid rectangle 12.0 mm (0.47 in) deep, sized against the 240 MPa minimum yield. Bending moment and design factor stay the same. This is a first-pass check, not a design allowable.

  1. Allowable ratio. A356.0-T61 test bars have a 180 MPa (26 ksi) minimum yield, so the section modulus must rise by 240 ÷ 180 = 1.333.
  2. New depth. For a rectangle of fixed width, section modulus grows with depth squared. Depth rises by √1.333 = 1.155, from 12.0 mm to 13.9 mm (0.55 in).
  3. New weight. With 2.67 g/cm³ for A356, that section weighs 1.155 × 2.67 ÷ 2.70 = 1.14 times as much, about 14% more.
  4. Body properties. On specimens cut from the casting, B108 keeps A356.0-T61 yield at 180 MPa, designated area or not, so depth stays 13.9 mm. Minimum tensile falls to 230 or 195 MPa (33 or 28 ksi).
  5. A357 instead. A357.0-T61 test bars, and specimens cut from a designated area, have a 250 MPa (36 ksi) minimum yield, so the 12.0 mm depth holds. With no location designated, yield is 215 MPa (31 ksi): depth becomes 12.0 × √(240 ÷ 215) = 12.7 mm (0.50 in), about 4% heavier. Minimum elongation falls to 3%.

The lesson: a material swap alone makes a strength-limited part heavier. Weight comes back only when the redesign uses the casting's shape freedom, or when the drawing sets agreed properties in the zones that carry the load.

When does a casting cost less than a billet part?

A casting usually wins when most of the bar would become chips and the annual volume pays for the tooling. Billet wins when quantities are small or the design still changes, because it needs no die.

Start with the buy-to-fly ratio: the mass of metal you buy divided by the mass of the finished part.

  • Take an illustrative housing that finishes at 0.85 kg (1.9 lb), cut from a 150 × 110 × 70 mm (5.9 × 4.3 × 2.8 in) block of 6061. The block is 1,155 cm³ × 2.70 g/cm³ = 3.12 kg (6.9 lb). The ratio is 3.7, and 73% of the bar leaves as chips.
  • Cast with machining stock on the functional faces, the same housing might weigh 0.95 kg (2.1 lb). The ratio drops to about 1.1. The heavy roughing passes disappear; finishing passes on the faces that matter remain.
Cost per part for the billet and casting routes
Cost elementBillet routeCasting route
MetalBar mass × bar price per kgCasting mass × casting price per kg
MachiningLong cycle, roughing plus finishing, × machine-hour rateShort cycle, finishing only, × machine-hour rate
InspectionDimensional checksDimensional checks plus any X-ray or leak test
ToolingFixtures onlyDie cost ÷ number of parts it will make

The break-even quantity is N = T ÷ (C_billet − C_cast), where T is the die cost and both unit costs leave the die out. Example in relative units: billet part 10, cast and finished part 4, die 3,000, so N = 3,000 ÷ 6 = 500 parts. N must fit inside the die life and the program volume.

Rows of blue racks filled with permanent molds in a tall, well-lit storage hall
Tooling storage area for permanent molds

Should a billet part become a casting? A decision table

If most lines fall in the right-hand column, ask for a drawing review.

When a machined billet part should become a casting
FactorLeans billet (machined bar or plate)Leans casting (heat-treated A356 or A357)
Annual volume and design statusPrototypes, small or uncertain volume, design still changingRepeat orders for years, design frozen
GeometryPrismatic shapes and open pockets a cutter can reachInternal passages, cored cavities, undercuts, curved forms
Part countOne simple partSeveral machined or welded pieces that could become one casting
Material removedStock already close to final shapeHigh buy-to-fly ratio; most of the bar becomes chips
Strength and ductility240 MPa (35 ksi) minimum yield or 10% elongation needed everywhereMet by A356.0-T61 or A357.0-T61 (ASTM B108) on the agreed test basis, or sized by stiffness
IntegrityNo porosity acceptance plan wantedX-ray zones and a leak test can be specified
TolerancesMost features tightMost features as cast; only interfaces machined
FinishDecorative anodizing requiredPaint or powder coat; EN 1706 rates the A356 type poor for decorative anodizing
TimingParts needed before a die could be madeProgram can wait for tooling and first-article approval

What changes on the drawing when a billet part becomes a casting?

The casting needs its own drawing. A billet drawing has no draft, sharp inside corners and tight tolerances on every face.

  • Alloy. Replace 6061-T6 with a casting alloy and temper, such as A356.0-T61 to ASTM B108. The A356 material page lists what the callout needs.
  • Draft. Add draft to walls parallel to the die opening; agree the angle with the foundry.
  • Fillets. Replace sharp inside corners with radii. Sharp corners raise stress and feed poorly.
  • Even walls. Replace thick blocks with walls and ribs of similar thickness. Heavy sections that solidify last are where shrinkage porosity forms.
  • Machining allowance. Add stock only to machined faces and keep as-cast datums for the first setup. ISO 8062-3:2023 sets casting tolerance grades and machining allowances.
  • Property zones. Mark the zones that carry load or pressure, with the required properties and how each is verified.

The gravity casting design guide covers draft, fillets, cores and wall layout.

How to write it into the drawing and RFQ

  1. Material line. Alloy, temper, standard, edition and unit system, for example A356.0-T61, ASTM B108/B108M-25, inch-pound limits. The SI limits are not exact conversions, so do not mix the two.
  2. Test basis. Separately cast test bars, specimens cut from the casting, or both, with the frequency and the lot definition. List the values to report, including yield strength when the design relies on it.
  3. Zone properties. The agreed tensile values for each critical zone and the specimen location.
  4. Integrity. The radiographic standard and grade per zone; the leak-test medium, pressure, hold time and acceptance.
  5. Dimensions. The as-cast tolerance standard and grade, and the list of machined features.
  6. Volumes. Annual quantity and expected program life, so the die steel can be chosen.

What inspection does a casting need that a billet part does not?

A casting can hold porosity that nobody sees until a cutter or a test finds it. A cast replacement on a pressure boundary or under cyclic load needs an inspection plan the billet part never had.

  • Pressure boundary. State the leak-test method, medium, pressure, hold time and acceptance, and whether impregnation is allowed. See the leak-test specification guide.
  • Fatigue zones. Name the radiographic reference standard and the grade for each zone, such as ASTM E155-20(2026), ASTM E2422-22 or GB/T 11346-2018. A grade in one system does not equal a grade in another.
  • Machined sealing faces. Say where exposed pores are not acceptable after machining. The porosity causes and detection guide explains the acceptance options.

At Bohua

We leak test by air-under-water immersion at 3 bar or more; when the drawing sets its own test pressure, we follow the drawing. Impregnation is used only with the customer's approval and is done by a qualified outside supplier. We inspect castings on Unicomp UNC-160 and Y.MU2000-D X-ray systems. Routine production typically meets GB/T 11346-2018 Grade 3–4; with tighter process control, sampled parts are around Grade 2; when the customer specifies it, every casting is X-rayed and shipped parts meet Grade 1.

Converting a billet part at Bohua

Send the current machined drawing with the loads, the annual volume and the faces that must stay machined. The drawing review is free.

At Bohua

Our engineers check which casting process suits the part and suggest where the design could change, once we know what the part must achieve. You decide which changes go into the drawing. Many of the parts we cast today went into production with changes we proposed. Only the review is free; tooling, samples and parts are quoted.

Four casting processes are in-house: gravity including tilt-pour, low-pressure, die casting on 280 t and 450 t machines, and sand casting. We design and make our dies in-house. Most are GB 45 carbon steel, which lasts about 20,000–50,000 cycles; H13 dies last about 100,000 cycles with scheduled maintenance. From drawing confirmation to first article takes 5–6 weeks. We cast A356 and ZL114 on our gravity and tilt-pour lines, with T5/T6 heat treatment and CNC machining on the same site. If your drawing calls out A357, send the specification for review.

Orders are quoted by annual volume; small batches are negotiable.

Vertical machining centers
16
CNC lathes
22
Drawing confirmation to first article
5–6 weeks
As-cast tolerance grade
CT8

The casting and CNC machining page lists the machining and inspection equipment. For the next step up in strength, see A356 vs A357; the closest Chinese grade to A357 is ZL114A, an approximate match.

Billet vs cast aluminum: buyer questions

Is billet aluminum stronger than cast aluminum?

In yield strength and elongation, yes. 6061-T6 extruded bar has minimums of 240 MPa (35 ksi) yield and 10% elongation; under ASTM B108/B108M-19, A356.0-T61 permanent-mold test bars have 180 MPa (26 ksi) and 4% (SI table) or 5% (inch-pound). Minimum tensile strength is about the same for both: 260 MPa in the SI tables and 38 ksi in the inch-pound tables. A357.0-T61 test bars reach 250 MPa (36 ksi) minimum yield, with 3% elongation.

Is billet or cast aluminum better?

Neither in general. Billet suits prototypes, small volumes and parts that need the most ductility. A casting suits repeat volumes, cored or curved shapes, and parts where most of the bar would be machined away.

Can the casting be made in 6061?

Not as a normal foundry route. 6061 is registered as a wrought alloy, so the casting drawing needs a registered casting alloy such as A356.0 or A357.0.

Will a cast part hold billet tolerances?

Only on machined features. As-cast surfaces follow a tolerance grade, such as a DCTG grade in ISO 8062-3:2023; name the standard, edition and grade on the drawing. At Bohua, as-cast dimensions hold CT8, or about DCTG 6 where needed (0.78 mm total for 63–100 mm). Critical machined dimensions can be held to ±0.02 mm, our limit; ±0.005 mm work is outside our capability.

Sources

  • Aluminum Association, Table 11.1, June 2017 page (extruded bar limits); Teal Sheets, August 2018 (6061 density).
  • ASTM B108/B108M-19 and B26/B26M-18.
  • ASTM B108/B108M-25, active edition (status and scope only).
  • EN 1706:2020+A1:2021, clause 7.3 and Annexes C and D.
  • GAG 001, Terms and Definitions, 2011.
  • Tajiri et al., Fracture and Structural Integrity, 2015 (A356-T6 fatigue).
  • Typical values: Kaiser Aluminum, Alloy 6061 technical data, Rev. 05/06; Rio Tinto foundry alloys, 2019; Rheinfelden Alloys handbook, 2016.

Get a free drawing review for your billet part

Include the machined drawing, annual volume, loads or pressure, and the faces that must stay machined. Submit the RFQ details, then email your drawing for review.

Send your drawing →

Linda

Export Sales

linda@ningbobohua.com

Ningbo, Zhejiang, China